Main Grade
Grade of high-quality alloy pipe :P1,P2,P5,P9,P11,P22,P91,P92 etc
Chemical Component
Grade |
UN |
C≤ |
Mn |
P≤ |
S≤ |
Si≤ |
Cr |
Mo |
Sequiv. |
P1 |
K11522 |
0.10~0.20 |
0.30~0.80 |
0.025 |
0.025 |
0.10~0.50 |
– |
0.44~0.65 |
P2 |
K11547 |
0.10~0.20 |
0.30~0.61 |
0.025 |
0.025 |
0.10~0.30 |
0.50~0.81 |
0.44~0.65 |
P5 |
K41545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
4.00~6.00 |
0.44~0.65 |
P5b |
K51545 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.00~2.00 |
4.00~6.00 |
0.44~0.65 |
P5c |
K41245 |
0.12 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
4.00~6.00 |
0.44~0.65 |
P9 |
S50400 |
0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.50~1.00 |
8.00~10.00 |
0.44~0.65 |
P11 |
K11597 |
0.05~0.15 |
0.30~0.61 |
0.025 |
0.025 |
0.50~1.00 |
1.00~1.50 |
0.44~0.65 |
P12 |
K11562 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
0.80~1.25 |
0.44~0.65 |
P15 |
K11578 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
1.15~1.65 |
– |
0.44~0.65 |
P21 |
K31545 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
2.65~3.35 |
0.80~1.60 |
P22 |
K21590 |
0.05~0.15 |
0.30~0.60 |
0.025 |
0.025 |
0.5 |
1.90~2.60 |
0.87~1.13 |
P91 |
K91560 |
0.08~0.12 |
0.30~0.60 |
0.02 |
0.01 |
0.20~0.50 |
8.00~9.50 |
0.85~1.05 |
P92 |
K92460 |
0.07~0.13 |
0.30~0.60 |
0.02 |
0.01 |
0.5 |
8.50~9.50 |
0.30~0.60 |
A New designation established in accordance with Practice E 527 and SAE J1086, Practice for Numbering Metals and Alloys (UNS). B Grade P 5c shall have a titanium content of not less than 4 times the carbon content and not more than 0.70 %; or a columbium content of 8 to 10 times the carbon content.
Mechanical Property
Mechanical properties |
P1,P2 |
P12 |
P23 |
P91 |
P92,P11 |
P122 |
Tensile strength |
380 |
415 |
510 |
585 |
620 |
620 |
Yield strength |
205 |
220 |
400 |
415 |
440 |
400 |
Heat Treatment
Grade |
Heat Treatment Type |
Normalizing Temperature Range F [C] |
Subcritical Annealing or Tempering |
P5, P9, P11, and P22 |
Temperature Range F [C] |
A335 P5 (b,c) |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1250 [675] |
|
Subcritical Anneal (P5c only) |
***** |
1325 – 1375 [715 - 745] |
A335 P9 |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1250 [675] |
A335 P11 |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1200 [650] |
A335 P22 |
Full or Isothermal Anneal |
|
|
|
Normalize and Temper |
***** |
1250 [675] |
A335 P91 |
Normalize and Temper |
1900-1975 [1040 - 1080] |
1350-1470 [730 - 800] |
|
Quench and Temper |
1900-1975 [1040 - 1080] |
1350-1470 [730 - 800] |
Test Requirement
In addition to ensuring chemical composition and mechanical properties, hydrostatic tests are performed one by one, Nondestructive Examination ,Product Analysis , Metal Structure and Etching Tests ,Flattening test etc.
Supply Ability
Supply Ability: 2000 Tons Per Month Per Grade of ASTM A335 Alloy Steel Pipe
Packaging
In Bundles And In Strong Wooden Box
Delivery
7-14 days if in stock, 30-45 days to produce
Payment
30% depsoit, 70% L/C or B/L copy or 100% L/C at sight
Product Detail
Boiler Tube
alloy steel pipehigh pressure boiler pipeseamless alloy steel pipe
Seamless steel tubes for high-pressure boilers ASTM A335/A335M-2018 Related Video: