Our development depends on the advanced equipment ,excellent talents and continuously strengthened technology forces for our high quality industry steel pipe, We are going to continually strive to increase our company and supply the ideal quality products with aggressive price ranges. Any inquiry or comment is hugely appreciated. Remember to get hold of us freely. Our company is working by the operation principle of "integrity-based, cooperation created, people oriented, win-win cooperation". We hope we can have a friendly relationship with businessman from all over the world
P91 not only has high oxidation resistance and high temperature steam corrosion resistance, but also has good impact toughness and high and stable long-lasting plasticity and thermal strength. When the service temperature is lower than 620℃, its allowable stress is higher than that of austenitic stainless steel. Above 550℃, the recommended design allowable stress is about twice that of T9 and 2.25Cr-1Mo steel. It can be used as high temperature superheater and reheater steel pipe for subcritical and supercritical boiler wall temperature ≤625℃, high temperature header and steam pipe wall temperature ≤600℃, as well as nuclear power heat exchanger and furnace tube of petroleum cracking unit.
It is mainly used to make high-quality alloy steel boiler pipe , heat exchanged pipe, high pressure steam pipe for petroleum and chemical industry
Grade of high-quality alloy pipe :P1,P2,P5,P9,P11,P22,P91,P92 etc
Grade | UN | C≤ | Mn | P≤ | S≤ | Si≤ | Cr | Mo |
Sequiv. | ||||||||
P1 | K11522 | 0.10~0.20 | 0.30~0.80 | 0.025 | 0.025 | 0.10~0.50 | – | 0.44~0.65 |
P2 | K11547 | 0.10~0.20 | 0.30~0.61 | 0.025 | 0.025 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 |
P5 | K41545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P5b | K51545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.00~2.00 | 4.00~6.00 | 0.44~0.65 |
P5c | K41245 | 0.12 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P9 | S50400 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.50~1.00 | 8.00~10.00 | 0.44~0.65 |
P11 | K11597 | 0.05~0.15 | 0.30~0.61 | 0.025 | 0.025 | 0.50~1.00 | 1.00~1.50 | 0.44~0.65 |
P12 | K11562 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 0.80~1.25 | 0.44~0.65 |
P15 | K11578 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.15~1.65 | – | 0.44~0.65 |
P21 | K31545 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 2.65~3.35 | 0.80~1.60 |
P22 | K21590 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 1.90~2.60 | 0.87~1.13 |
P91 | K91560 | 0.08~0.12 | 0.30~0.60 | 0.02 | 0.01 | 0.20~0.50 | 8.00~9.50 | 0.85~1.05 |
P92 | K92460 | 0.07~0.13 | 0.30~0.60 | 0.02 | 0.01 | 0.5 | 8.50~9.50 | 0.30~0.60 |
A New designation established in accordance with Practice E 527 and SAE J1086, Practice for Numbering Metals and Alloys (UNS). B Grade P 5c shall have a titanium content of not less than 4 times the carbon content and not more than 0.70 %; or a columbium content of 8 to 10 times the carbon content.
Mechanical properties | P1,P2 | P12 | P23 | P91 | P92,P11 | P122 |
Tensile strength | 380 | 415 | 510 | 585 | 620 | 620 |
Yield strength | 205 | 220 | 400 | 415 | 440 | 400 |
Grade | Heat Treatment Type | Normalizing Temperature Range F [C] | Subcritical Annealing or Tempering |
P5, P9, P11, and P22 | Temperature Range F [C] | ||
A335 P5 (b,c) | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
Subcritical Anneal (P5c only) | ***** | 1325 – 1375 [715 - 745] | |
A335 P9 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P11 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1200 [650] | |
A335 P22 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P91 | Normalize and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Quench and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
In addition to ensuring chemical composition and mechanical properties, hydrostatic tests are performed one by one, Nondestructive Examination ,Product Analysis , Metal Structure and Etching Tests ,Flattening test etc.
Supply Ability: 2000 Tons Per Month Per Grade of ASTM A335 Alloy Steel Pipe
In Bundles And In Strong Wooden Box
7-14 days if in stock, 30-45 days to produce
30% depsoit, 70% L/C or B/L copy or 100% L/C at sight