Our organization puts emphasis to the administration, the introduction of talented personnel, and also the construction of team building, making an attempt hard to enhance the standard and liability consciousness of workers members. Our business successfully attained IS9001 Certification and European CE Certification of A335 High Pressure Boiler Heat Exchange Alloy Seamless Steel Pipe, We play a leading role in furnishing clients with good quality goods great provider and aggressive charges. Create Values,Serving Customer!" is the aim we pursue. We sincerely hope that all customers will establish long term and mutually beneficial cooperation with us.If you wish to get more details about our company, Be sure to contact with us now!
It is mainly used to make high-quality alloy steel boiler pipe , heat exchanged pipe, high pressure steam pipe for petroleum and chemical industry
Grade of high-quality alloy pipe :P1,P2,P5,P9,P11,P22,P91,P92 etc
Grade | UN | C≤ | Mn | P≤ | S≤ | Si≤ | Cr | Mo |
Sequiv. | ||||||||
P1 | K11522 | 0.10~0.20 | 0.30~0.80 | 0.025 | 0.025 | 0.10~0.50 | – | 0.44~0.65 |
P2 | K11547 | 0.10~0.20 | 0.30~0.61 | 0.025 | 0.025 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 |
P5 | K41545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P5b | K51545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.00~2.00 | 4.00~6.00 | 0.44~0.65 |
P5c | K41245 | 0.12 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P9 | S50400 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.50~1.00 | 8.00~10.00 | 0.44~0.65 |
P11 | K11597 | 0.05~0.15 | 0.30~0.61 | 0.025 | 0.025 | 0.50~1.00 | 1.00~1.50 | 0.44~0.65 |
P12 | K11562 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 0.80~1.25 | 0.44~0.65 |
P15 | K11578 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.15~1.65 | – | 0.44~0.65 |
P21 | K31545 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 2.65~3.35 | 0.80~1.60 |
P22 | K21590 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 1.90~2.60 | 0.87~1.13 |
P91 | K91560 | 0.08~0.12 | 0.30~0.60 | 0.02 | 0.01 | 0.20~0.50 | 8.00~9.50 | 0.85~1.05 |
P92 | K92460 | 0.07~0.13 | 0.30~0.60 | 0.02 | 0.01 | 0.5 | 8.50~9.50 | 0.30~0.60 |
A New designation established in accordance with Practice E 527 and SAE J1086, Practice for Numbering Metals and Alloys (UNS). B Grade P 5c shall have a titanium content of not less than 4 times the carbon content and not more than 0.70 %; or a columbium content of 8 to 10 times the carbon content.
Mechanical properties | P1,P2 | P12 | P23 | P91 | P92,P11 | P122 |
Tensile strength | 380 | 415 | 510 | 585 | 620 | 620 |
Yield strength | 205 | 220 | 400 | 415 | 440 | 400 |
Grade | Heat Treatment Type | Normalizing Temperature Range F [C] | Subcritical Annealing or Tempering |
P5, P9, P11, and P22 | Temperature Range F [C] | ||
A335 P5 (b,c) | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
Subcritical Anneal (P5c only) | ***** | 1325 – 1375 [715 - 745] | |
A335 P9 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P11 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1200 [650] | |
A335 P22 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P91 | Normalize and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Quench and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
In addition to ensuring chemical composition and mechanical properties, hydrostatic tests are performed one by one, Nondestructive Examination ,Product Analysis , Metal Structure and Etching Tests ,Flattening test etc.
Supply Ability: 2000 Tons Per Month Per Grade of ASTM A335 Alloy Steel Pipe